1. Hadawa
Idan aka kwatanta da nau'ikan robar chloroprene na gargajiya. Polyethylene mai chlorine ba ya buƙatar plasticization kuma baya buƙatar ajiya bayan plasticization. Ana iya motsa ƙarin sifofi na ruwa a cikin dabarar polyethylene mai chlorine kuma a sha ta wasu foda yayin aikin batching, wanda zai iya guje wa tsaftacewa da digowa yayin aikin haɗawa na ainihi. Ana buƙatar zafin vulcanization na polyethylene mai chlorine ya wuce 160 ℃ Ana iya ci gaba da samarwa da ruwan sanyaya, amma zafin jiki gabaɗaya baya wuce 160 ℃. Don haka wakilin vulcanizing da ake amfani da shi a cikin polyethylene mai chlorine ba ya buƙatar a ƙara shi daban da sauran ƙari, kuma ana iya haɗa shi kai tsaye da sauran foda. Bukatun zafin haɗuwa don polyethylene mai chlorine suna da faɗi kaɗan, daga 40 ℃ zuwa 120 ℃, kuma ba za a sami mannewa ko ƙone na'urorin ba. Lokacin amfani da mahaɗin buɗewa, yana da mahimmanci a kashe ruwan sanyaya ko kunna tururin a kan lokaci. Saboda polyethylene mai chlorine yana samar da isasshen kuzarin zafi saboda gogayya yayin haɗawa, yana da mahimmanci a ƙara isasshen ruwan sanyaya lokacin haɗawa a cikin mahaɗin ciki. Zafin rarrabawa gabaɗaya yana tsakanin ℃ 110 zuwa ℃ 120 Wannan yana ba da damar yin aiki mai yawa na haɗawa ba tare da yin mummunan tasiri ga ingancin polyethylene mai chlorine ba.
2. Ajiye motoci da gyaran zafi
Idan aka kwatanta da robar chloroprene, robar gauraye ta polyethylene mai chlorine tana da kwanciyar hankali a ajiya kuma ba ta buƙatar adanawa a ƙarancin zafin jiki. Yanayin zafi mai yawa a lokacin rani ba ya shafar ta kai tsaye. Polyethylene mai chlorine ba ya buƙatar sanyaya yayin tacewa mai zafi, kuma zafin tacewa gabaɗaya yana sama da 50 ℃.
3. Yin murfin kariya ga wayoyi da kebul
Ana iya amfani da polyethylene mai sinadarin chlorine wajen samar da murfin waya da kebul ta amfani da dogayen kayan fitar da sukurori ko kuma gajerun kayan fitar da sukurori. Gabaɗaya, murfin waya da kebul da masu fitar da sukurori masu dogon zango suka yi zai yi haske, ya yi laushi, kuma yana da cikakkun sassan giciye. Lokacin fitar da manne na polyethylene mai sinadarin chlorine, zafin kan gaba ɗaya yana tsakanin 6 ° C da 90 ° C. Saboda tsananin zafi da ke tattare da gogayya yayin aikin tace polyethylene mai sinadarin chlorine, zafin da ke cikin robar zai fi girma, gabaɗaya tsakanin 90 ° C da 120 ° C. Saboda haka, lokacin amfani da mai fitar da sukurori mai dogon zango, ya zama dole a sa ido da kuma sarrafa zafin jiki na asali sosai don guje wa ƙone kayan roba.
4. Tsarin haɗa sinadarin sulfur
Idan aka kwatanta da sauran nau'ikan kayan roba da aka saba amfani da su, zafin da ake buƙata don tsarin vulcanization na polyethylene mai chlorine yana da yawa, yawanci tsakanin 160 ℃ da 180 ℃ Bukatun vulcanization don waya mai chlorine da robar kebul sune:; Lokacin da matsin lamba mai cike da tururi ya kai 054 MPa, zafin vulcanization shine 160 ℃ kuma lokacin vulcanization yawanci yana tsakanin minti 25 zuwa minti 30. Lokacin da matsin lamba mai cike da tururi ya kai 098MFRa, zafin vulcanization shine 180 ℃ kuma lokacin vulcanization yawanci yana tsakanin minti 6-10. Lokacin da matsin lamba mai cike da tururi ya kai 152MPa, zafin vulcanization shine 200 ℃ kuma lokacin vulcanization yawanci yana tsakanin minti 1-3. Yayin da matsin lamba mai cike da tururi ya ƙaru a hankali, zafin vulcanization kuma yana ƙaruwa a hankali, yayin da lokacin vulcanization ya ragu. Sakamakon robar polyethylene mai chlorine yana da juriya mafi kyau ga tsagewa.
Lokacin Saƙo: Yuli-05-2025